Euclid Hi-Flow Metallic Grout is a high-tolerance, non-shrink metallic-aggregate grout for extra-heavy machinery, columns, crane rails, and bearing plates. The shrinkage-compensating binder stays highly fluid without bleeding.
Euclid Hi-Flow Metallic Grout is a high-tolerance, non-shrink cementitious grout with metallic aggregate and a shrinkage-compensating binder for extra-heavy machinery, crane rails, bridge seats, and bearing plates. It places at a fluid consistency without bleeding, then hardens under extra-heavy equipment. Euclid lists it chloride-free, with rapid strength gain for equipment re-grouts.
| Property | Value |
|---|---|
| 28-day compressive, fluid | 9,000 psi |
| 1-day compressive, fluid | 4,000 psi |
| 7-day compressive, fluid | 7,000 psi |
| Volume change | +0.03% |
| Initial set | 3 hr 50 min |
| Final set | 4 hr 50 min |
| Placement temperature | 40 to 100 F |
| Compliance | ASTM C1107, CRD-C 621 |
| Yield | 0.40 ft³ per 50 lb |
| Documents | Hi-Flow Metallic Grout TDS |
When should I use Euclid Hi-Flow Metallic Grout?
Euclid Hi-Flow Metallic Grout is for heavy duty grouting of machinery and equipment, structural columns, crane rails, bridge seats, and bearing plates. Euclid formulated it as a metallic aggregate system for extra heavy duty service conditions.
When do I pick Euclid Hi-Flow Metallic Grout instead of Euclid Hi-Flow Grout?
Euclid Hi-Flow Metallic Grout is a metallic aggregate system for extra heavy duty service. Euclid Hi-Flow Grout is a natural aggregate system. Pick Metallic when the job needs metallic aggregate under extra-heavy machinery, crane rails, or bearing plates.
What compressive strength does Euclid Hi-Flow Metallic Grout reach?
Under laboratory conditions at fluid consistency, Euclid publishes 4,000 psi at 1 day, 6,000 psi at 3 days, 7,000 psi at 7 days, and 9,000 psi at 28 days (ASTM C109M, 2 in cubes). Expect reasonable variation under field conditions.
What specifications does Euclid Hi-Flow Metallic Grout meet?
Euclid publishes Hi-Flow Metallic Grout to CRD-C 621 and ASTM C1107.
What does Euclid Hi-Flow Metallic Grout publish about chlorides?
Euclid publishes that Hi-Flow Metallic Grout does not contain any chlorides or additives which may contribute to corrosion of the base structure.
What temperature range is Euclid Hi-Flow Metallic Grout designed for fluid placement?
Euclid publishes Hi-Flow Metallic Grout as designed to be fluid poured at 40 to 100 F.